15-5PH / X5CrNiCuNb15-5 vs X5CrNiMo17-12-2: 50% composition overlap. Moderate differences, generally not direct substitutes.

15-5PH / X5CrNiCuNb15-5 vs X5CrNiMo17-12-2

Side-by-side chemical composition and mechanical property comparison.

Overview

15-5PH / X5CrNiCuNb15-5

1.4545

Stainless Steelph

Martensitic precipitation-hardening stainless steel. Similar to 17-4PH but with better transverse ductility and toughness due to lower delta ferrite. Used for aerospace structural components, nuclear reactor parts, food processing equipment, and high-performance fasteners.

X5CrNiMo17-12-2

1.4401

Stainless SteelAustenitic

Standard molybdenum-bearing austenitic stainless steel, known as AISI 316. Similar to 1.4404 (316L) but with higher carbon content (max 0.07%) providing slightly better high-temperature strength. Not resistant to intergranular corrosion after welding β€” for welded constructions prefer 1.4404 (316L). Used in chemical processing, marine environments, and applications requiring improved pitting resistance over 1.4301 (304).

15-5PH / X5CrNiCuNb15-5X5CrNiMo17-12-2
Material Number1.45451.4401
CategoryStainless SteelStainless Steel
StandardAMS 5659EN 10088-3

Chemical composition (wt%)

Element15-5PH / X5CrNiCuNb15-5X5CrNiMo17-12-2Overlap
C0–0.07%≀ 0.07%OK
Si0–1%≀ 1%OK
Mn0–1%≀ 2%OK
P0–0.03%β€”β€”

Mechanical properties

Property15-5PH / X5CrNiCuNb15-5X5CrNiMo17-12-2Unit
tensile_strengthβ‰₯ 1310β€”MPa
yield_strengthβ‰₯ 1170β€”MPa
elongationβ‰₯ 10β€”%

Compatibility Assessment

15-5PH / X5CrNiCuNb15-5 and X5CrNiMo17-12-2 have moderate differences (50% overlap). They are generally not direct substitutes. Consider the specific requirements of your application.

Automated assessment based on composition analysis

Frequently Asked Questions

Is 15-5PH / X5CrNiCuNb15-5 the same as X5CrNiMo17-12-2?

15-5PH / X5CrNiCuNb15-5 and X5CrNiMo17-12-2 have a 50% composition overlap. They are generally not directly interchangeable.

Can I replace 15-5PH / X5CrNiCuNb15-5 with X5CrNiMo17-12-2?

Generally not recommended. The compositions differ significantly (50% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between 15-5PH / X5CrNiCuNb15-5 and X5CrNiMo17-12-2?

The main differences are in the following elements: Cr, Ni. 15-5PH / X5CrNiCuNb15-5 is a Stainless Steel grade, while X5CrNiMo17-12-2 is a Stainless Steel grade.