EN AW-2024 vs EN AC-AlSi7Mg0.3: 16% composition overlap. Significantly different materials serving different application areas.
EN AW-2024 vs EN AC-AlSi7Mg0.3
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-2024
3.1355
Classic high-strength aerospace aluminium alloy (Al-Cu-Mg). Excellent fatigue resistance β the standard choice for aircraft fuselage skins and wing tension members. Poor corrosion resistance and weldability. Often supplied with Alclad cladding for corrosion protection. In use since 1931.
EN AC-AlSi7Mg0.3
EN AC-42100
The most important aluminum sand and gravity die casting alloy worldwide. Excellent castability, good mechanical properties after T6 heat treatment, and outstanding weldability. Si 6.5-7.5% provides excellent fluidity, Mg 0.25-0.45% enables precipitation hardening. Used for automotive wheels, suspension components, aerospace structural castings, engine brackets, and high-integrity safety-critical castings. Equivalent to ASTM A356.0 and DIN G-AlSi7Mg.
| EN AW-2024 | EN AC-AlSi7Mg0.3 | |
|---|---|---|
| Material Number | 3.1355 | EN AC-42100 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 1706 |
Chemical composition (wt%)
| Element | EN AW-2024 | EN AC-AlSi7Mg0.3 | Overlap |
|---|---|---|---|
| Si | 0β0.5% | 6.5β7.5% | No overlap |
| Mn | 0.3β0.9% | β€ 0.1% | No overlap |
| Cr | 0β0.1% | β | β |
| Cu | 3.8β4.9% | β€ 0.05% | No overlap |
Mechanical properties
| Property | EN AW-2024 | EN AC-AlSi7Mg0.3 | Unit |
|---|---|---|---|
| tensile_strength | 400β430 | β₯ 140 | MPa |
| yield_strength | 270β280 | β₯ 80 | MPa |
| elongation | β₯ 10 | β₯ 2 | % |
Compatibility Assessment
EN AW-2024 and EN AC-AlSi7Mg0.3 have significantly different compositions (16% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-2024 the same as EN AC-AlSi7Mg0.3?
EN AW-2024 and EN AC-AlSi7Mg0.3 have a 16% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-2024 with EN AC-AlSi7Mg0.3?
Generally not recommended. The compositions differ significantly (16% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-2024 and EN AC-AlSi7Mg0.3?
The main differences are in the following elements: Si, Mn, Cu, Mg. EN AW-2024 is a Aluminum grade, while EN AC-AlSi7Mg0.3 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.