EN AW-2024 vs EN AW-5356: 33% composition overlap. Significantly different materials serving different application areas.
EN AW-2024 vs EN AW-5356
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-2024
3.1355
Classic high-strength aerospace aluminium alloy (Al-Cu-Mg). Excellent fatigue resistance β the standard choice for aircraft fuselage skins and wing tension members. Poor corrosion resistance and weldability. Often supplied with Alclad cladding for corrosion protection. In use since 1931.
EN AW-5356
EN AW-5356
THE magnesium-aluminum welding filler wire β Mg 4.5-5.5% + Cr 0.05-0.20%. Together with 4043, accounts for the vast majority of all Al welding wire sold. ER5356/AlMg5Cr(A). Better color match after anodizing than 4043 (no dark spots). Higher weld strength than 4043. Used for MIG/TIG welding of 5xxx and 6xxx base alloys. THE filler for marine, structural, and anodized applications.
| EN AW-2024 | EN AW-5356 | |
|---|---|---|
| Material Number | 3.1355 | EN AW-5356 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | AWS A5.10 |
Chemical composition (wt%)
| Element | EN AW-2024 | EN AW-5356 | Overlap |
|---|---|---|---|
| Si | 0β0.5% | 0β0.25% | OK |
| Mn | 0.3β0.9% | 0.05β0.2% | No overlap |
| Cr | 0β0.1% | 0.05β0.2% | Partial |
| Cu | 3.8β4.9% | β | β |
Mechanical properties
| Property | EN AW-2024 | EN AW-5356 | Unit |
|---|---|---|---|
| tensile_strength | 400β430 | 245β285 | MPa |
| yield_strength | 270β280 | 120β165 | MPa |
| elongation | β₯ 10 | 17β25 | % |
Compatibility Assessment
EN AW-2024 and EN AW-5356 have significantly different compositions (33% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-2024 the same as EN AW-5356?
EN AW-2024 and EN AW-5356 have a 33% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-2024 with EN AW-5356?
Generally not recommended. The compositions differ significantly (33% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-2024 and EN AW-5356?
The main differences are in the following elements: Mn, Cr, Ti, Mg. EN AW-2024 is a Aluminum grade, while EN AW-5356 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.