Skip to content
Automated comparison Β· 49% overlap

310S / X8CrNi25-21 vs Super Duplex 2507: 49% composition overlap. Significantly different materials serving different application areas.

310S / X8CrNi25-21 vs Super Duplex 2507

Side-by-side chemical composition and mechanical property comparison.

Sign up free for 3 comparisons per daySign up β†’

Overview

310S / X8CrNi25-21

1.4845

Stainless SteelAustenitic

High-chromium, high-nickel austenitic for the highest service temperatures among standard austenitics. Oxidation resistance to ~1100Β°C (continuous). Higher Cr/Ni than 309S. Used for furnace parts, radiant tubes, heat treatment baskets, kiln liners, and high-temperature flue gas equipment.

Super Duplex 2507

1.4410

Stainless SteelDuplex

Super duplex stainless steel with PREN >40. Superior corrosion resistance to standard 2205 duplex, especially in chloride and Hβ‚‚S environments. Used for subsea pipelines, offshore platform components, desalination plants, and chemical processing equipment.

310S / X8CrNi25-21Super Duplex 2507
Material Number1.48451.4410
CategoryStainless SteelStainless Steel
StandardEN 10088-2EN 10088-2

Chemical composition (wt%) β€” Pro

Element310S / X8CrNi25-21Super Duplex 2507Overlap
C0–0.1%0–0.03%OK
Si0–1.5%0–0.8%OK
Mn0–2%0–1.2%OK
Pβ€”0–0.035%β€”
S
Cr
Mo
Ni
N

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Mechanical properties β€” Pro

Property310S / X8CrNi25-21Super Duplex 2507Unit
Tensile Strength500–700730–930MPa
Yield Strengthβ‰₯ 210β‰₯ 530MPa
Elongationβ‰₯ 35β‰₯ 20%
Elastic Modulus
Density
Hardness HB

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Compatibility Assessment

310S / X8CrNi25-21 and Super Duplex 2507 have significantly different compositions (49% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is 310S / X8CrNi25-21 the same as Super Duplex 2507?

310S / X8CrNi25-21 and Super Duplex 2507 have a 49% composition overlap. They are generally not directly interchangeable.

Can I replace 310S / X8CrNi25-21 with Super Duplex 2507?

Generally not recommended. The compositions differ significantly (49% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between 310S / X8CrNi25-21 and Super Duplex 2507?

The main differences are in the following elements: Ni. 310S / X8CrNi25-21 is a Stainless Steel grade, while Super Duplex 2507 is a Stainless Steel grade.

Related Comparisons

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.