Skip to content
Automated comparison Β· 44% overlap

316Ti vs X2CrNiMoN25-7-4: 44% composition overlap. Significantly different materials serving different application areas.

316Ti vs X2CrNiMoN25-7-4

Side-by-side chemical composition and mechanical property comparison.

Overview

316Ti

1.4571

Stainless SteelAustenitic

Titanium-stabilized austenitic stainless steel with molybdenum. Stabilization prevents sensitization during prolonged high-temperature exposure. Very popular in Germany for chemical, pharmaceutical, and food processing. Being replaced internationally by 316L (1.4404) for most applications.

X2CrNiMoN25-7-4

1.4410

Stainless SteelDuplex

Super duplex stainless steel (SAF 2507 / UNS S32750) with 25% Cr, 7% Ni, 4% Mo, and high N for PREN β‰₯42. The highest corrosion resistance and strength among standard duplex grades β€” YS β‰₯550 MPa is ~2.5Γ— that of 316L. Service temperature up to 300Β°C. Used for subsea oil & gas equipment (manifolds, trees, risers), desalination plants, flue gas cleaning, chemical tankers, and mining equipment in severe chloride environments. Requires careful welding to avoid sigma phase.

316TiX2CrNiMoN25-7-4
Material Number1.45711.4410
CategoryStainless SteelStainless Steel
StandardEN 10088-2EN 10088-2

Chemical composition (wt%)

Element316TiX2CrNiMoN25-7-4Overlap
C0–0.08%≀ 0.03%OK
Si0–1%≀ 0.8%OK
Mn0–2%≀ 1.2%OK
P0–0.045%≀ 0.035%OK

Mechanical properties

Property316TiX2CrNiMoN25-7-4Unit
tensile_strength500–700800–1000MPa
yield_strengthβ‰₯ 200β‰₯ 550MPa
elongationβ‰₯ 40β‰₯ 15%

Compatibility Assessment

316Ti and X2CrNiMoN25-7-4 have significantly different compositions (44% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is 316Ti the same as X2CrNiMoN25-7-4?

316Ti and X2CrNiMoN25-7-4 have a 44% composition overlap. They are generally not directly interchangeable.

Can I replace 316Ti with X2CrNiMoN25-7-4?

Generally not recommended. The compositions differ significantly (44% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between 316Ti and X2CrNiMoN25-7-4?

The main differences are in the following elements: Cr, Mo, Ni. 316Ti is a Stainless Steel grade, while X2CrNiMoN25-7-4 is a Stainless Steel grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.