EN AW-5182

3.3519

Aluminum5xxx_mg

One of the strongest non-heat-treatable Al-Mg alloys. 4.5% Mg + 0.35% Mn. THE standard alloy for beverage can lids/pull tabs (H48 temper). Also used for automotive body panels (hoods, doors), fuel tanks, and marine components. Excellent corrosion resistance and formability.

EN AW-6061

3.3211

Aluminum6xxx_mg_si

THE US structural aluminum alloy β€” AlMg1SiCu. Good strength (UTS 290 T6), excellent corrosion resistance, and good weldability. THE default choice in North America for structural and machined parts. Cu addition gives slightly better strength than 6082 in some tempers but slightly worse corrosion. Used for structural frames, bicycle frames, aircraft fittings, marine hardware, and general machined components.

EN AW-5182EN AW-6061
Material Number3.35193.3211
CategoryAluminumAluminum
StandardEN 573-3EN 755-2

Chemical composition (wt%) β€” Pro

ElementEN AW-5182EN AW-6061Overlap
Si0–0.2%0.4–0.8%No overlap
Mn0.2–0.5%0–0.15%No overlap
Cr0–0.1%0.04–0.35%Partial
Cu0–0.15%0.15–0.4%Partial
Al
Ti
Mg
Fe
Zn

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Mechanical properties β€” Pro

PropertyEN AW-5182EN AW-6061Unit
Tensile Strength275–330260–310MPa
Yield Strength130–190240–275MPa
Elongation20–258–12%
Elastic Modulus
Density
Hardness HB
Tensile Strength
Yield Strength Rp0.2
Elongation A
Hardness HB
Density

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Compatibility Assessment

EN AW-5182 and EN AW-6061 have significantly different compositions (37% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-5182 the same as EN AW-6061?

EN AW-5182 and EN AW-6061 have a 37% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-5182 with EN AW-6061?

Generally not recommended. The compositions differ significantly (37% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5182 and EN AW-6061?

The main differences are in the following elements: Si, Mn, Cr, Cu. EN AW-5182 is a Aluminum grade, while EN AW-6061 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.