EN AW-7050 vs EN AW-5356: 22% composition overlap. Significantly different materials serving different application areas.
EN AW-7050 vs EN AW-5356
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-7050
3.4144
High-strength aerospace aluminium developed by Alcoa for thick-plate applications. Zr addition (instead of Cr) reduces quench sensitivity for superior properties in thick sections. T7451 temper gives excellent SCC resistance + fracture toughness. Used for fuselage frames, bulkheads, wing spars, and thick structural aerospace components.
EN AW-5356
EN AW-5356
THE magnesium-aluminum welding filler wire β Mg 4.5-5.5% + Cr 0.05-0.20%. Together with 4043, accounts for the vast majority of all Al welding wire sold. ER5356/AlMg5Cr(A). Better color match after anodizing than 4043 (no dark spots). Higher weld strength than 4043. Used for MIG/TIG welding of 5xxx and 6xxx base alloys. THE filler for marine, structural, and anodized applications.
| EN AW-7050 | EN AW-5356 | |
|---|---|---|
| Material Number | 3.4144 | EN AW-5356 |
| Category | Aluminum | Aluminum |
| Standard | AMS 4050 | AWS A5.10 |
Chemical composition (wt%)
| Element | EN AW-7050 | EN AW-5356 | Overlap |
|---|---|---|---|
| Si | 0β0.12% | 0β0.25% | OK |
| Mn | 0β0.1% | 0.05β0.2% | Partial |
| Cr | β | 0.05β0.2% | β |
| Cu | 2β2.6% | β | β |
Mechanical properties
| Property | EN AW-7050 | EN AW-5356 | Unit |
|---|---|---|---|
| tensile_strength | β₯ 510 | 245β285 | MPa |
| yield_strength | β₯ 450 | 120β165 | MPa |
| elongation | β₯ 9 | 17β25 | % |
Compatibility Assessment
EN AW-7050 and EN AW-5356 have significantly different compositions (22% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-7050 the same as EN AW-5356?
EN AW-7050 and EN AW-5356 have a 22% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-7050 with EN AW-5356?
Generally not recommended. The compositions differ significantly (22% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-7050 and EN AW-5356?
The main differences are in the following elements: Mn, Ti, Mg. EN AW-7050 is a Aluminum grade, while EN AW-5356 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.