E7018-1 H4R vs ER308L: 46% composition overlap. Significantly different materials serving different application areas.

E7018-1 H4R vs ER308L

Side-by-side chemical composition and mechanical property comparison.

Overview

E7018-1 H4R

WeldingStick (SMAW)

Low-hydrogen basic coated SMAW electrode with enhanced toughness (-45Β°C) and moisture-resistant coating (H4R designation = max 4ml Hβ‚‚/100g, moisture-resistant). The premium structural steel electrode for critical applications: bridges, high-rise buildings, offshore structures, pressure vessels (ASME Section IX) and seismic-resistant frames. 70 ksi (485 MPa) tensile strength. AC or DCEP. The "-1" suffix indicates 27J impact at -45Β°C. H4R coating resists moisture pickup for 9+ hours after removal from hermetically sealed packaging.

ER308L

WeldingSolid Wire (MIG/TIG)

Low-carbon austenitic stainless steel welding wire β€” the standard filler for joining 304 and 304L stainless steels. The L (low carbon ≀0.03%) prevents sensitization and intergranular corrosion in the heat-affected zone. Used for TIG (GTAW) and MIG (GMAW) with pure argon or Ar/CO2 shielding. Produces fully austenitic-ferritic weld metal with 5-15 FN (Ferrite Number) for crack resistance. Used for food processing equipment, chemical tanks, pharmaceutical vessels, and architectural stainless fabrication.

E7018-1 H4RER308L
Material Numberβ€”β€”
CategoryWeldingWelding
StandardAWS A5.1AWS A5.9

Chemical composition (wt%)

ElementE7018-1 H4RER308LOverlap
C≀ 0.08%≀ 0.03%OK
Si0.3–0.6%0.3–0.65%OK
Mn1–1.6%1–2.5%OK
P≀ 0.025%≀ 0.03%OK

Mechanical properties

PropertyE7018-1 H4RER308LUnit
Tensile Strengthβ‰₯ 485β€”MPa
Yield Strengthβ‰₯ 400β€”MPa
Elongationβ‰₯ 22β€”%

Compatibility Assessment

E7018-1 H4R and ER308L have significantly different compositions (46% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is E7018-1 H4R the same as ER308L?

E7018-1 H4R and ER308L have a 46% composition overlap. They are generally not directly interchangeable.

Can I replace E7018-1 H4R with ER308L?

Generally not recommended. The compositions differ significantly (46% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between E7018-1 H4R and ER308L?

The main differences are in the following elements: Cr, Ni. E7018-1 H4R is a Welding grade, while ER308L is a Welding grade.

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.