Skip to content
Automated comparison Β· 43% overlap

EN-GJL-200 vs EN-GJL-350: 43% composition overlap. Significantly different materials serving different application areas.

EN-GJL-200 vs EN-GJL-350

Side-by-side chemical composition and mechanical property comparison.

Sign up free for 3 comparisons per daySign up β†’

Overview

EN-GJL-200

0.6020

Alloy Steelgrey_cast_iron

Grey cast iron with lamellar graphite and minimum tensile strength 200 MPa. Ferrite-pearlite matrix. Good balance of castability, machinability, and moderate strength. Excellent vibration damping. The most economical grey iron grade for general engineering. Used for machine bases, pump housings, valve bodies, pipe fittings, brake drums, and general-purpose castings. Equivalent to DIN GG20 and ASTM A48 Class 30.

EN-GJL-350

0.6035

Alloy Steelgrey_cast_iron

Grey cast iron with lamellar graphite and minimum tensile strength 350 MPa. The highest standard strength grade. Fully pearlitic or even bainitic matrix with possible alloying (Cr, Cu, Ni) to achieve high strength. Reduced machinability compared to lower grades. Used for heavy-duty cylinder liners, large diesel engine blocks, high-performance brake discs, press frames, and heavily loaded machine components. Equivalent to DIN GG35 and ASTM A48 Class 50.

EN-GJL-200EN-GJL-350
Material Number0.60200.6035
CategoryAlloy SteelAlloy Steel
StandardEN 1561EN 1561

Chemical composition (wt%) β€” Pro

ElementEN-GJL-200EN-GJL-350Overlap
C3–3.3%2.5–2.9%No overlap
Si1.5–2.2%1–1.4%No overlap
Mn0.6–0.9%0.8–1.2%Partial
P≀ 0.15%≀ 0.15%OK
S

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Mechanical properties β€” Pro

PropertyEN-GJL-200EN-GJL-350Unit
Tensile Strengthβ‰₯ 200β‰₯ 350MPa
Hardness HB160–210228–285HB
Densityβ‰₯ 7.15β‰₯ 7.3g/cm3
Thermal Conductivity
Elastic Modulus

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Compatibility Assessment

EN-GJL-200 and EN-GJL-350 have significantly different compositions (43% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN-GJL-200 the same as EN-GJL-350?

EN-GJL-200 and EN-GJL-350 have a 43% composition overlap. They are generally not directly interchangeable.

Can I replace EN-GJL-200 with EN-GJL-350?

Generally not recommended. The compositions differ significantly (43% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN-GJL-200 and EN-GJL-350?

The main differences are in the following elements: C, Si, Mn. EN-GJL-200 is a Alloy Steel grade, while EN-GJL-350 is a Alloy Steel grade.

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.