Hastelloy C-22 vs Hastelloy C-276: Same family β C-22 has more Cr for better oxidizing resistance
Hastelloy C-22 vs Hastelloy C-276
Side-by-side chemical composition and mechanical property comparison.
Overview
Hastelloy C-22
2.4602
Improved version of Hastelloy C-276 with better resistance to oxidizing media and higher chromium. Considered the most versatile Ni-Cr-Mo alloy for chemical processing. Resists both oxidizing and reducing acids, chlorides, and mixed media. Used for flue gas desulfurization, pharmaceutical, and universal chemical processing.
Hastelloy C-276
2.4819
The most versatile corrosion-resistant alloy available. Ni-Mo-Cr-W composition resists both oxidizing and reducing environments. Outstanding resistance to pitting, stress corrosion cracking, and wet chlorine gas. Used in chemical processing, flue gas desulfurization, pulp & paper, and waste treatment.
| Hastelloy C-22 | Hastelloy C-276 | |
|---|---|---|
| Material Number | 2.4602 | 2.4819 |
| Category | Nickel Alloys | Nickel Alloys |
| Standard | ASTM B575 | ASTM B575 |
Chemical composition (wt%)
| Element | Hastelloy C-22 | Hastelloy C-276 | Overlap |
|---|---|---|---|
| C | 0β0.01% | 0β0.01% | OK |
| Si | 0β0.08% | 0β0.08% | OK |
| Mn | 0β0.5% | 0β1% | OK |
| Cr | 20β22.5% | 14.5β16.5% | No overlap |
Mechanical properties
| Property | Hastelloy C-22 | Hastelloy C-276 | Unit |
|---|---|---|---|
| tensile_strength | β₯ 690 | β₯ 690 | MPa |
| yield_strength | β₯ 310 | β₯ 310 | MPa |
| elongation | β₯ 45 | β₯ 40 | % |
Compatibility Assessment
C-22 has higher Cr (20-22.5% vs 14.5-16.5%) for superior oxidizing environment resistance. C-276 has more Mo (15-17% vs 12.5-14.5%) for better reducing acid resistance. C-22 increasingly preferred as the universal grade.
Frequently Asked Questions
Is Hastelloy C-22 the same as Hastelloy C-276?
Hastelloy C-22 and Hastelloy C-276 have a 85% composition overlap. Same family β C-22 has more Cr for better oxidizing resistance
Can I replace Hastelloy C-22 with Hastelloy C-276?
In many cases, yes. The compositions overlap significantly (85%). However, always verify mechanical property requirements and heat treatment compatibility for your specific application.
What is the difference between Hastelloy C-22 and Hastelloy C-276?
The main differences are in the following elements: Cr, Mo, W, Fe. Hastelloy C-22 is a Nickel Alloys grade, while Hastelloy C-276 is a Nickel Alloys grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.