Skip to content

CuSn6

CW452K
Copper & Brassphosphor_bronze
Compare with…Export PDF

Phosphor bronze with 6% tin — better cold formability than CuSn8 at slightly lower strength. Excellent spring properties and fatigue resistance. Used for electrical connectors, spring contacts, switch parts, bellows, bourdon tubes, and precision springs.

International equivalents

FlagStandardCountryGradeNumberMatch
🇺🇸UNSUSAUNS C51900C51900REF
🇪🇺ENEuropeCuSn6CW452K100%

Sources: ASTM B103, EN 1652

Chemical composition comparison (wt%)

Side-by-side: CuSn6 (EN) (EN 1652) vs CuSn6 (EN) (EN 1652)

ElementCuSn6 (EN)CuSn6 (EN)Overlap
P0.01–0.4%0.01–0.4%OK
Ni0–0.3%0–0.3%OK
Cu———
Sn5.5–7%5.5–7%OK
Zn0–0.3%0–0.3%OK
Pb0–0.02%0–0.02%OK
Fe0–0.1%0–0.1%OK

Mechanical properties

R420

PropertyValueUnit
Tensile Strength420–520MPa
Yield Strength≥ 280MPa
Elongation≥ 18%
Elastic Modulus≥ 110GPa
Density≥ 8.8g/cm3