P295GH
1.0481Mid-range pressure vessel steel — ReH >=295 MPa. Between P265GH and P355GH. Used for unfired pressure vessels, heat exchangers, and boiler components per EN 10028-2. Good weldability and guaranteed elevated-temperature yield strength. Widely specified in European process plant design.
International equivalents
| Flag | Standard | Country | Grade | Number | Match |
|---|---|---|---|---|---|
| 🇪🇺 | EN | Europe | P295GH / 1.0481 | 1.0481 | 100% |
Sources: EN 10028-2
Chemical composition comparison (wt%)
Side-by-side: P295GH (EN 10028-2) vs P295GH / 1.0481 (EN) (EN 10028-2)
| Element | P295GH (EN 10028-2) | P295GH / 1.0481 (EN) | Overlap |
|---|---|---|---|
| C | — | 0–0.2% | — |
| Si | — | 0–0.4% | — |
Mechanical properties
Compatibility verdict
P295GH and P295GH / 1.0481: 100% composition match
Related materials
C45
1.0503Medium carbon unalloyed quality steel. Good machinability and moderate strength after heat treatment. Widely used for shafts, spindles, pins, studs, and general machine parts.
S355JR
1.0045High-strength low-alloy structural steel with minimum yield strength of 355 MPa. Standard grade for bridges, buildings, cranes, and general structural applications. Impact tested at +20°C (JR).
S235JR
1.0038General-purpose structural steel with minimum yield strength of 235 MPa. The most common structural steel grade in Europe for general construction, frames, and non-critical structural applications.
Export this comparison as PDF
Professional datasheet with equivalents, composition, and properties. Ready for your QM documentation.
Download PDF — €4.90Included with PRO subscription