S275N
1.0490Normalized fine-grain structural steel with 275 MPa yield. The lowest strength grade in the EN 10025-3 normalized series. Better weldability and guaranteed fine-grain structure compared to standard S275JR. Used for welded structures, bridges, and general steelwork where normalized delivery is specified.
International equivalents
| Flag | Standard | Country | Grade | Number | Match |
|---|---|---|---|---|---|
| 🇪🇺 | EN | Europe | S275N | 1.0490 | 100% |
Sources: EN 10025-3:2019
Chemical composition comparison (wt%)
Side-by-side: S275N (EN 10025-3) vs S275N (EN) (EN 10025-3:2019)
| Element | S275N (EN 10025-3) | S275N (EN) | Overlap |
|---|---|---|---|
| C | — | 0–0.16% | — |
| Si | — | 0–0.4% | — |
Mechanical properties
Compatibility verdict
S275N and S275N: 100% composition match
Related materials
C45
1.0503Medium carbon unalloyed quality steel. Good machinability and moderate strength after heat treatment. Widely used for shafts, spindles, pins, studs, and general machine parts.
S355JR
1.0045High-strength low-alloy structural steel with minimum yield strength of 355 MPa. Standard grade for bridges, buildings, cranes, and general structural applications. Impact tested at +20°C (JR).
S235JR
1.0038General-purpose structural steel with minimum yield strength of 235 MPa. The most common structural steel grade in Europe for general construction, frames, and non-critical structural applications.
Export this comparison as PDF
Professional datasheet with equivalents, composition, and properties. Ready for your QM documentation.
Download PDF — €4.90Included with PRO subscription