EN AW-5083 vs EN AW-5182: Both high-Mg 5xxx alloys β different application domains
EN AW-5083 vs EN AW-5182
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5083
3.3547
The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).
EN AW-5182
3.3519
One of the strongest non-heat-treatable Al-Mg alloys. 4.5% Mg + 0.35% Mn. THE standard alloy for beverage can lids/pull tabs (H48 temper). Also used for automotive body panels (hoods, doors), fuel tanks, and marine components. Excellent corrosion resistance and formability.
| EN AW-5083 | EN AW-5182 | |
|---|---|---|
| Material Number | 3.3547 | 3.3519 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-5083 | EN AW-5182 | Overlap |
|---|---|---|---|
| Si | 0β0.4% | 0β0.2% | OK |
| Mn | 0.4β1% | 0.2β0.5% | Partial |
| Cr | 0.05β0.25% | 0β0.1% | Partial |
| Cu | 0β0.1% | 0β0.15% | OK |
Mechanical properties
| Property | EN AW-5083 | EN AW-5182 | Unit |
|---|---|---|---|
| tensile_strength | 275β350 | 275β330 | MPa |
| yield_strength | β₯ 125 | 130β190 | MPa |
| elongation | β₯ 12 | 20β25 | % |
Compatibility Assessment
5083 is stronger (UTS 310-450 vs 275-330 for 5182) and is THE marine structural alloy. 5182 has better formability and is THE beverage can lid alloy. Choose 5083 for structural marine/pressure vessels; 5182 for deep-drawn packaging and automotive body panels.
Frequently Asked Questions
Is EN AW-5083 the same as EN AW-5182?
EN AW-5083 and EN AW-5182 have a 70% composition overlap. Both high-Mg 5xxx alloys β different application domains
Can I replace EN AW-5083 with EN AW-5182?
In many cases, yes. The compositions overlap significantly (70%). However, always verify mechanical property requirements and heat treatment compatibility for your specific application.
What is the difference between EN AW-5083 and EN AW-5182?
The main differences are in the following elements: Mn, Cr. EN AW-5083 is a Aluminum grade, while EN AW-5182 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.