EN AW-6082 vs EN AW-5083: Different aluminium alloy families β€” heat-treatable vs non-heat-treatable

EN AW-6082 vs EN AW-5083

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-6082

3.2315

Aluminum6xxx (Al-Mg-Si)

High-strength structural aluminium alloy in the Al-Mg-Si family. One of the strongest 6xxx series alloys due to manganese addition. Replaced 6061 in many European applications. Used for trusses, bridges, cranes, transport, scaffolding, and marine applications. Heat treatable (T6/T651).

EN AW-5083

3.3547

Aluminum5xxx (Al-Mg)

The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).

EN AW-6082EN AW-5083
Material Number3.23153.3547
CategoryAluminumAluminum
StandardEN 573-3EN 573-3

Chemical composition (wt%)

ElementEN AW-6082EN AW-5083Overlap
Si0.7–1.3%0–0.4%No overlap
Mn0.4–1%0.4–1%OK
Cr0–0.25%0.05–0.25%OK
Cu0–0.1%0–0.1%OK

Mechanical properties

PropertyEN AW-6082EN AW-5083Unit
tensile_strengthβ‰₯ 310275–350MPa
yield_strengthβ‰₯ 260β‰₯ 125MPa
elongationβ‰₯ 8β‰₯ 12%

Compatibility Assessment

6082 is Al-Mg-Si (heat-treatable, higher strength in T6). 5083 is Al-Mg (non-heat-treatable, superior corrosion/welding). Choose 6082 for structural strength, 5083 for marine/welded applications.

Frequently Asked Questions

Is EN AW-6082 the same as EN AW-5083?

EN AW-6082 and EN AW-5083 have a 30% composition overlap. Different aluminium alloy families β€” heat-treatable vs non-heat-treatable

Can I replace EN AW-6082 with EN AW-5083?

Generally not recommended. The compositions differ significantly (30% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-6082 and EN AW-5083?

The main differences are in the following elements: Si, Mg. EN AW-6082 is a Aluminum grade, while EN AW-5083 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.