Skip to content
Automated comparison Β· 15% overlap

EN AW-5083 vs EN AW-7050: 15% composition overlap. Significantly different materials serving different application areas.

EN AW-5083 vs EN AW-7050

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-5083

3.3547

Aluminum5xxx (Al-Mg)

The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).

EN AW-7050

3.4144

Aluminum7xxx (Al-Zn)

High-strength aerospace aluminium developed by Alcoa for thick-plate applications. Zr addition (instead of Cr) reduces quench sensitivity for superior properties in thick sections. T7451 temper gives excellent SCC resistance + fracture toughness. Used for fuselage frames, bulkheads, wing spars, and thick structural aerospace components.

EN AW-5083EN AW-7050
Material Number3.35473.4144
CategoryAluminumAluminum
StandardEN 573-3AMS 4050

Chemical composition (wt%)

ElementEN AW-5083EN AW-7050Overlap
Si0–0.4%0–0.12%OK
Mn0.4–1%0–0.1%No overlap
Cr0.05–0.25%β€”β€”
Cu0–0.1%2–2.6%No overlap

Mechanical properties

PropertyEN AW-5083EN AW-7050Unit
tensile_strength275–350β‰₯ 510MPa
yield_strengthβ‰₯ 125β‰₯ 450MPa
elongationβ‰₯ 12β‰₯ 9%

Compatibility Assessment

EN AW-5083 and EN AW-7050 have significantly different compositions (15% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-5083 the same as EN AW-7050?

EN AW-5083 and EN AW-7050 have a 15% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-5083 with EN AW-7050?

Generally not recommended. The compositions differ significantly (15% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5083 and EN AW-7050?

The main differences are in the following elements: Mn, Cu, Mg, Zn. EN AW-5083 is a Aluminum grade, while EN AW-7050 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.