EN AW-5083 vs EN AC-AlSi10Mg: 38% composition overlap. Significantly different materials serving different application areas.
EN AW-5083 vs EN AC-AlSi10Mg
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5083
3.3547
The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).
EN AC-AlSi10Mg
EN AC-43000
Versatile aluminum casting alloy with excellent castability and good mechanical properties. THE standard alloy for metal 3D printing (SLM/DMLS/L-PBF) due to its excellent processability with laser powder bed fusion. Also widely used in conventional sand casting and gravity die casting. Si 9-11% provides outstanding fluidity and low shrinkage. Used for automotive structural parts, aerospace components, 3D-printed functional prototypes and series parts, heat exchangers, and complex thin-walled castings.
| EN AW-5083 | EN AC-AlSi10Mg | |
|---|---|---|
| Material Number | 3.3547 | EN AC-43000 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 1706 |
Chemical composition (wt%)
| Element | EN AW-5083 | EN AC-AlSi10Mg | Overlap |
|---|---|---|---|
| Si | 0β0.4% | 9β11% | No overlap |
| Mn | 0.4β1% | β€ 0.45% | Partial |
| Cr | 0.05β0.25% | β | β |
| Cu | 0β0.1% | β€ 0.05% | OK |
Mechanical properties
| Property | EN AW-5083 | EN AC-AlSi10Mg | Unit |
|---|---|---|---|
| tensile_strength | 275β350 | β₯ 150 | MPa |
| yield_strength | β₯ 125 | β₯ 80 | MPa |
| elongation | β₯ 12 | β₯ 2 | % |
Compatibility Assessment
EN AW-5083 and EN AC-AlSi10Mg have significantly different compositions (38% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5083 the same as EN AC-AlSi10Mg?
EN AW-5083 and EN AC-AlSi10Mg have a 38% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5083 with EN AC-AlSi10Mg?
Generally not recommended. The compositions differ significantly (38% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5083 and EN AC-AlSi10Mg?
The main differences are in the following elements: Si, Mn, Mg. EN AW-5083 is a Aluminum grade, while EN AC-AlSi10Mg is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.