Skip to content
Automated comparison Β· 37% overlap

EN AW-5083 vs EN AW-3003: 37% composition overlap. Significantly different materials serving different application areas.

EN AW-5083 vs EN AW-3003

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-5083

3.3547

Aluminum5xxx (Al-Mg)

The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).

EN AW-3003

EN AW-3003

Aluminum3xxx_al_mn

Al-Mn general purpose alloy β€” Mn 1.0-1.5%. ~20% stronger than 1100 pure Al with similar excellent formability, corrosion resistance, and weldability. Non-heat-treatable. THE cooking/food industry aluminum: pots, pans, beverage cans, heat exchangers, chemical equipment, and general sheet metal. Also used for roofing, siding, and storage tanks.

EN AW-5083EN AW-3003
Material Number3.3547EN AW-3003
CategoryAluminumAluminum
StandardEN 573-3EN 573-3

Chemical composition (wt%)

ElementEN AW-5083EN AW-3003Overlap
Si0–0.4%0–0.6%OK
Mn0.4–1%1–1.5%Partial
Cr0.05–0.25%β€”β€”
Cu0–0.1%0.05–0.2%Partial

Mechanical properties

PropertyEN AW-5083EN AW-3003Unit
tensile_strength275–350140–175MPa
yield_strengthβ‰₯ 125115–145MPa
elongationβ‰₯ 124–8%

Compatibility Assessment

EN AW-5083 and EN AW-3003 have significantly different compositions (37% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-5083 the same as EN AW-3003?

EN AW-5083 and EN AW-3003 have a 37% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-5083 with EN AW-3003?

Generally not recommended. The compositions differ significantly (37% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5083 and EN AW-3003?

The main differences are in the following elements: Mn, Cu. EN AW-5083 is a Aluminum grade, while EN AW-3003 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.