Overview
EN AW-5083
3.3547
The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).
EN AW-3004
EN AW-3004
Al-Mn-Mg alloy β THE beverage can body material. Mn 1.0-1.5% + Mg 0.8-1.3% give moderate strength (UTS 240-280 H19) with excellent formability for deep drawing and ironing. ~200 billion cans/year worldwide. Also used for roofing sheet, color-coated panels, and storage tanks. Stronger than 3003 due to Mg addition.
| EN AW-5083 | EN AW-3004 | |
|---|---|---|
| Material Number | 3.3547 | EN AW-3004 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-5083 | EN AW-3004 | Overlap |
|---|---|---|---|
| Si | 0β0.4% | 0β0.3% | OK |
| Mn | 0.4β1% | 1β1.5% | Partial |
| Cr | 0.05β0.25% | β | β |
| Cu | 0β0.1% | β | β |
Mechanical properties
| Property | EN AW-5083 | EN AW-3004 | Unit |
|---|---|---|---|
| tensile_strength | 275β350 | 230β270 | MPa |
| yield_strength | β₯ 125 | 190β230 | MPa |
| elongation | β₯ 12 | 5β9 | % |
Compatibility Assessment
EN AW-5083 and EN AW-3004 have significantly different compositions (33% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5083 the same as EN AW-3004?
EN AW-5083 and EN AW-3004 have a 33% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5083 with EN AW-3004?
Generally not recommended. The compositions differ significantly (33% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5083 and EN AW-3004?
The main differences are in the following elements: Mn, Mg. EN AW-5083 is a Aluminum grade, while EN AW-3004 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.