EN AW-5083 vs EN AW-5356: 52% composition overlap. Moderate differences, generally not direct substitutes.
EN AW-5083 vs EN AW-5356
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5083
3.3547
The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).
EN AW-5356
EN AW-5356
THE magnesium-aluminum welding filler wire β Mg 4.5-5.5% + Cr 0.05-0.20%. Together with 4043, accounts for the vast majority of all Al welding wire sold. ER5356/AlMg5Cr(A). Better color match after anodizing than 4043 (no dark spots). Higher weld strength than 4043. Used for MIG/TIG welding of 5xxx and 6xxx base alloys. THE filler for marine, structural, and anodized applications.
| EN AW-5083 | EN AW-5356 | |
|---|---|---|
| Material Number | 3.3547 | EN AW-5356 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | AWS A5.10 |
Chemical composition (wt%)
| Element | EN AW-5083 | EN AW-5356 | Overlap |
|---|---|---|---|
| Si | 0β0.4% | 0β0.25% | OK |
| Mn | 0.4β1% | 0.05β0.2% | No overlap |
| Cr | 0.05β0.25% | 0.05β0.2% | OK |
| Cu | 0β0.1% | β | β |
Mechanical properties
| Property | EN AW-5083 | EN AW-5356 | Unit |
|---|---|---|---|
| tensile_strength | 275β350 | 245β285 | MPa |
| yield_strength | β₯ 125 | 120β165 | MPa |
| elongation | β₯ 12 | 17β25 | % |
Compatibility Assessment
EN AW-5083 and EN AW-5356 have moderate differences (52% overlap). They are generally not direct substitutes. Consider the specific requirements of your application.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5083 the same as EN AW-5356?
EN AW-5083 and EN AW-5356 have a 52% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5083 with EN AW-5356?
Generally not recommended. The compositions differ significantly (52% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5083 and EN AW-5356?
The main differences are in the following elements: Mn, Ti, Mg. EN AW-5083 is a Aluminum grade, while EN AW-5356 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.