EN AW-5754 vs EN AW-5356: 48% composition overlap. Significantly different materials serving different application areas.
EN AW-5754 vs EN AW-5356
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5754
3.3535
Medium-strength non-heat-treatable aluminium alloy with good corrosion resistance and excellent weldability. Lower Mg than 5083 for better formability. The standard alloy for automotive body panels (inner), chemical equipment, and food industry applications.
EN AW-5356
EN AW-5356
THE magnesium-aluminum welding filler wire β Mg 4.5-5.5% + Cr 0.05-0.20%. Together with 4043, accounts for the vast majority of all Al welding wire sold. ER5356/AlMg5Cr(A). Better color match after anodizing than 4043 (no dark spots). Higher weld strength than 4043. Used for MIG/TIG welding of 5xxx and 6xxx base alloys. THE filler for marine, structural, and anodized applications.
| EN AW-5754 | EN AW-5356 | |
|---|---|---|
| Material Number | 3.3535 | EN AW-5356 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | AWS A5.10 |
Chemical composition (wt%)
| Element | EN AW-5754 | EN AW-5356 | Overlap |
|---|---|---|---|
| Si | 0β0.4% | 0β0.25% | OK |
| Mn | 0β0.5% | 0.05β0.2% | OK |
| Cr | 0β0.3% | 0.05β0.2% | OK |
| Cu | 0β0.1% | β | β |
Mechanical properties
| Property | EN AW-5754 | EN AW-5356 | Unit |
|---|---|---|---|
| tensile_strength | 190β240 | 245β285 | MPa |
| yield_strength | β₯ 80 | 120β165 | MPa |
| elongation | β₯ 17 | 17β25 | % |
Compatibility Assessment
EN AW-5754 and EN AW-5356 have significantly different compositions (48% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5754 the same as EN AW-5356?
EN AW-5754 and EN AW-5356 have a 48% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5754 with EN AW-5356?
Generally not recommended. The compositions differ significantly (48% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5754 and EN AW-5356?
The main differences are in the following elements: Ti, Mg. EN AW-5754 is a Aluminum grade, while EN AW-5356 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.