Skip to content
Expert verdict Β· 65% match

EN AW-5083 vs EN AW-5754: Both 5xxx marine alloys β€” 5083 much stronger, 5754 more formable

EN AW-5083 vs EN AW-5754

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-5083

3.3547

Aluminum5xxx_mg

The highest-strength non-heat-treatable aluminum alloy. Al-Mg4.5-Mn with outstanding seawater and industrial chemical resistance. Retains exceptional strength after welding (unlike 6xxx/7xxx). ASTM B928 certified for marine service. THE shipbuilding aluminum β€” also used for rail cars, pressure vessels, cryogenic tanks, truck bodies, and LNG applications. Available O, H111, H116, H321 tempers.

EN AW-5754

3.3535

Aluminum5xxx (Al-Mg)

Medium-strength non-heat-treatable aluminium alloy with good corrosion resistance and excellent weldability. Lower Mg than 5083 for better formability. The standard alloy for automotive body panels (inner), chemical equipment, and food industry applications.

EN AW-5083EN AW-5754
Material Number3.35473.3535
CategoryAluminumAluminum
StandardEN 485-2EN 573-3

Chemical composition (wt%)

ElementEN AW-5083EN AW-5754Overlap
Si0–0.4%0–0.4%OK
Mn0.4–1%0–0.5%Partial
Cr0.05–0.25%0–0.3%OK
Cu0–0.1%0–0.1%OK

Mechanical properties

PropertyEN AW-5083EN AW-5754Unit
tensile_strength270–345190–240MPa
yield_strength115–130β‰₯ 80MPa
elongationβ‰₯ 16β‰₯ 17%

Compatibility Assessment

5083 has 4.5% Mg (UTS 305 H321) vs 5754 with 3% Mg (UTS 245 H22). 5083 is the strongest non-heat-treatable Al and the default for ship hulls. 5754 is easier to form and less susceptible to stress corrosion at elevated temperatures. Choose 5083 for structural marine; 5754 for automotive/formed parts.

Frequently Asked Questions

Is EN AW-5083 the same as EN AW-5754?

EN AW-5083 and EN AW-5754 have a 65% composition overlap. Both 5xxx marine alloys β€” 5083 much stronger, 5754 more formable

Can I replace EN AW-5083 with EN AW-5754?

Generally not recommended. The compositions differ significantly (65% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5083 and EN AW-5754?

The main differences are in the following elements: Mn, Mg. EN AW-5083 is a Aluminum grade, while EN AW-5754 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.