EN AW-6063 vs EN AW-6082: Same 6xxx family β 6063 for surface, 6082 for strength
EN AW-6063 vs EN AW-6082
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-6063
3.3206
The most common extrusion alloy worldwide. Excellent surface finish, good corrosion resistance, and exceptional extrudability. The standard choice for architectural profiles (window frames, curtain walls, railings), heat sinks, and electrical enclosures.
EN AW-6082
3.2315
High-strength structural aluminium alloy in the Al-Mg-Si family. One of the strongest 6xxx series alloys due to manganese addition. Replaced 6061 in many European applications. Used for trusses, bridges, cranes, transport, scaffolding, and marine applications. Heat treatable (T6/T651).
| EN AW-6063 | EN AW-6082 | |
|---|---|---|
| Material Number | 3.3206 | 3.2315 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-6063 | EN AW-6082 | Overlap |
|---|---|---|---|
| Si | 0.2β0.6% | 0.7β1.3% | No overlap |
| Mn | 0β0.1% | 0.4β1% | No overlap |
| Cr | 0β0.1% | 0β0.25% | OK |
| Cu | 0β0.1% | 0β0.1% | OK |
Mechanical properties
| Property | EN AW-6063 | EN AW-6082 | Unit |
|---|---|---|---|
| tensile_strength | β₯ 215 | β₯ 310 | MPa |
| yield_strength | β₯ 170 | β₯ 260 | MPa |
| elongation | β₯ 8 | β₯ 8 | % |
Compatibility Assessment
6063 has better extrudability and surface finish (ideal for architectural profiles). 6082 has significantly higher strength (310 vs 215 MPa UTS in T6). Choose 6063 for appearance, 6082 for structural load-bearing.
Frequently Asked Questions
Is EN AW-6063 the same as EN AW-6082?
EN AW-6063 and EN AW-6082 have a 60% composition overlap. Same 6xxx family β 6063 for surface, 6082 for strength
Can I replace EN AW-6063 with EN AW-6082?
Generally not recommended. The compositions differ significantly (60% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-6063 and EN AW-6082?
The main differences are in the following elements: Si, Mn, Mg. EN AW-6063 is a Aluminum grade, while EN AW-6082 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.