Skip to content
Automated comparison Β· 43% overlap

EN AW-7050 vs EN AW-5052: 43% composition overlap. Significantly different materials serving different application areas.

EN AW-7050 vs EN AW-5052

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-7050

3.4144

Aluminum7xxx (Al-Zn)

High-strength aerospace aluminium developed by Alcoa for thick-plate applications. Zr addition (instead of Cr) reduces quench sensitivity for superior properties in thick sections. T7451 temper gives excellent SCC resistance + fracture toughness. Used for fuselage frames, bulkheads, wing spars, and thick structural aerospace components.

EN AW-5052

EN AW-5052

Aluminum5xxx_al_mg

General-purpose Al-Mg alloy β€” Mg 2.2-2.8%. Good balance of formability, corrosion resistance, and moderate strength (UTS 210-260 H32). Non-heat-treatable β€” strengthened by cold work. THE most widely used 5xxx alloy globally by tonnage. Used for sheet metal work, fuel tanks, marine components, appliances, lighting, and general fabrication. Excellent weldability.

EN AW-7050EN AW-5052
Material Number3.4144EN AW-5052
CategoryAluminumAluminum
StandardAMS 4050EN 573-3

Chemical composition (wt%)

ElementEN AW-7050EN AW-5052Overlap
Si0–0.12%0–0.25%OK
Mn0–0.1%β€”β€”
Crβ€”0.15–0.35%β€”
Cu2–2.6%β€”β€”

Mechanical properties

PropertyEN AW-7050EN AW-5052Unit
tensile_strengthβ‰₯ 510210–260MPa
yield_strengthβ‰₯ 450160–210MPa
elongationβ‰₯ 97–12%

Compatibility Assessment

EN AW-7050 and EN AW-5052 have significantly different compositions (43% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-7050 the same as EN AW-5052?

EN AW-7050 and EN AW-5052 have a 43% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-7050 with EN AW-5052?

Generally not recommended. The compositions differ significantly (43% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-7050 and EN AW-5052?

The main differences are in the following elements: Mg. EN AW-7050 is a Aluminum grade, while EN AW-5052 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.