Waspaloy vs Inconel 718: Both age-hardenable superalloys β different temperature ranges
Waspaloy vs Inconel 718
Side-by-side chemical composition and mechanical property comparison.
Overview
Waspaloy
2.4654
Nickel-based gamma-prime strengthened superalloy β THE turbine disc material. Excellent creep-rupture strength up to 650Β°C (rotating) and 870Β°C (static). Developed 1950s by Pratt & Whitney. Triple-aged (solution + stabilize + precipitation) for peak properties. Superior to Inconel 718 above 650Β°C. Used for compressor and rotor discs, shafts, spacers, seals, rings, casings, and fasteners in gas turbine engines.
Inconel 718
2.4668
THE most widely used aerospace superalloy. Precipitation-hardened Ni-Cr-Fe alloy strengthened by gamma-prime and gamma-double-prime phases (Nb). Unique slow aging kinetics allow welding without cracking. UTS >1275 MPa aged. Used for gas turbine discs, jet engine components, rocket motors, cryogenic tanks, and oil/gas downhole tools. Service to 700Β°C.
| Waspaloy | Inconel 718 | |
|---|---|---|
| Material Number | 2.4654 | 2.4668 |
| Category | Nickel Alloys | Nickel Alloys |
| Standard | ASTM B637 | ASTM B637 |
Chemical composition (wt%)
| Element | Waspaloy | Inconel 718 | Overlap |
|---|---|---|---|
| C | 0.02β0.1% | 0β0.08% | Partial |
| Si | 0β0.75% | 0β0.35% | OK |
| Mn | 0β1% | 0β0.35% | OK |
| Cr | 18β21% | 17β21% | OK |
Mechanical properties
| Property | Waspaloy | Inconel 718 | Unit |
|---|---|---|---|
| tensile_strength | 1170β1310 | β₯ 1275 | MPa |
| yield_strength | 720β895 | β₯ 1034 | MPa |
| elongation | 15β25 | β₯ 12 | % |
Compatibility Assessment
Inconel 718 is stronger at room temp (UTS 1240 vs 1170 MPa typ) and much easier to weld. Waspaloy has superior creep-rupture above 650Β°C and better thermal stability. Choose 718 up to 650Β°C (easier/cheaper); Waspaloy above 650Β°C for rotating parts.
Frequently Asked Questions
Is Waspaloy the same as Inconel 718?
Waspaloy and Inconel 718 have a 55% composition overlap. Both age-hardenable superalloys β different temperature ranges
Can I replace Waspaloy with Inconel 718?
Generally not recommended. The compositions differ significantly (55% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between Waspaloy and Inconel 718?
The main differences are in the following elements: C, Mo, Al, Ti. Waspaloy is a Nickel Alloys grade, while Inconel 718 is a Nickel Alloys grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.