Skip to content

25CrS4

1.7036
Alloy SteelQuenched & Tempered
Compare with…Export PDF

Free-cutting variant of 25Cr4 — S 0.020-0.040%. Low-C Cr QT steel for CNC automatics. Good combination of machinability, moderate strength (UTS 750-900 MPa), and toughness. Used for bolts, studs, shafts, and automotive components where Cr-only hardenability with machinability is needed at lower cost than CrMo grades.

Chemical composition comparison (wt%)

Side-by-side: 25CrS4 (EN) (EN 10083-3) vs ASTM

Element25CrS4 (EN)ASTMOverlap
C0.22–0.29%——
Si0–0.4%——
Mn0.6–0.9%——
S0.02–0.04%——
Cr0.9–1.2%——

Mechanical properties

QT

PropertyValueUnit
Tensile Strength750–900MPa
Yield Strength500–650MPa
Elongation13–17%
Elastic Modulus≥ 210GPa
Density≥ 7.85g/cm3