Skip to content

CuNi2Be (CW110C)

CW110C
Copper & Brasscu_ni_be
Compare with…Export PDF

Nickel-beryllium copper alloy, precipitation hardened. Higher strength than CuBe2 (CW101C) with better thermal conductivity. Age-hardened: Rm 690–850 MPa, Rp0.2 550–750 MPa, HB 200–280. Electrical conductivity ~50–60% IACS. Non-sparking. UNS C17510, EN CW110C. Applications: plastic injection mold inserts (core pins), resistance welding electrodes (for coated steel), springs, connectors, non-sparking tools, blow mold inserts.

International equivalents

FlagStandardCountryGradeNumberMatch
🇪🇺ENEuropeCuNi2BeCW110C%
🇺🇸UNSUSAC17510%
🇩🇪DINGermanyCuNi2Be2.0850%
🇺🇸MaterionUSAAlloy 3%

Sources: CEN/TS 13388, UNS, DIN, materion.com

Chemical composition comparison (wt%)

Side-by-side: CuNi2Be (CW110C) (EN 12163 / CEN/TS 13388) vs CuNi2Be (EN) (CEN/TS 13388)

ElementCuNi2Be (CW110C) (EN 12163 / CEN/TS 13388)CuNi2Be (EN)Overlap
Ni1.4–2.2%
Cu≥ 96%

Mechanical properties

Compatibility verdict

CuNi2Be (CW110C) and CuNi2Be: null% composition match