EN AW-5083

3.3547

Aluminum5xxx (Al-Mg)

The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65Β°C under stress (SCC risk).

EN AW-6063

3.3206

Aluminum6xxx (Al-Mg-Si)

The most common extrusion alloy worldwide. Excellent surface finish, good corrosion resistance, and exceptional extrudability. The standard choice for architectural profiles (window frames, curtain walls, railings), heat sinks, and electrical enclosures.

EN AW-5083EN AW-6063
Material Number3.35473.3206
CategoryAluminumAluminum
StandardEN 573-3EN 573-3

Chemical composition (wt%) β€” Pro

ElementEN AW-5083EN AW-6063Overlap
Si0–0.4%0.2–0.6%Partial
Mn0.4–1%0–0.1%No overlap
Cr0.05–0.25%0–0.1%Partial
Cu0–0.1%0–0.1%OK
Ti
Fe
Mg
Zn

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Mechanical properties β€” Pro

PropertyEN AW-5083EN AW-6063Unit
Tensile Strength275–350β‰₯ 215MPa
Yield Strengthβ‰₯ 125β‰₯ 170MPa
Elongationβ‰₯ 12β‰₯ 8%
Elastic Modulus
Density
Hardness HB

Sign up free and get 3 full comparisons immediately.

Sign up free β€” 3 comparisons/day free

Compatibility Assessment

EN AW-5083 and EN AW-6063 have significantly different compositions (43% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-5083 the same as EN AW-6063?

EN AW-5083 and EN AW-6063 have a 43% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-5083 with EN AW-6063?

Generally not recommended. The compositions differ significantly (43% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5083 and EN AW-6063?

The main differences are in the following elements: Si, Mn, Cr, Mg. EN AW-5083 is a Aluminum grade, while EN AW-6063 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.