EN AW-5182 vs EN AW-6082: 46% composition overlap. Significantly different materials serving different application areas.
EN AW-5182 vs EN AW-6082
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5182
3.3519
One of the strongest non-heat-treatable Al-Mg alloys. 4.5% Mg + 0.35% Mn. THE standard alloy for beverage can lids/pull tabs (H48 temper). Also used for automotive body panels (hoods, doors), fuel tanks, and marine components. Excellent corrosion resistance and formability.
EN AW-6082
3.2315
High-strength structural aluminium alloy in the Al-Mg-Si family. One of the strongest 6xxx series alloys due to manganese addition. Replaced 6061 in many European applications. Used for trusses, bridges, cranes, transport, scaffolding, and marine applications. Heat treatable (T6/T651).
| EN AW-5182 | EN AW-6082 | |
|---|---|---|
| Material Number | 3.3519 | 3.2315 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-5182 | EN AW-6082 | Overlap |
|---|---|---|---|
| Si | 0β0.2% | 0.7β1.3% | No overlap |
| Mn | 0.2β0.5% | 0.4β1% | Partial |
| Cr | 0β0.1% | 0β0.25% | OK |
| Cu | 0β0.15% | 0β0.1% | OK |
Mechanical properties
| Property | EN AW-5182 | EN AW-6082 | Unit |
|---|---|---|---|
| tensile_strength | 275β330 | β₯ 310 | MPa |
| yield_strength | 130β190 | β₯ 260 | MPa |
| elongation | 20β25 | β₯ 8 | % |
Compatibility Assessment
EN AW-5182 and EN AW-6082 have significantly different compositions (46% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5182 the same as EN AW-6082?
EN AW-5182 and EN AW-6082 have a 46% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5182 with EN AW-6082?
Generally not recommended. The compositions differ significantly (46% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5182 and EN AW-6082?
The main differences are in the following elements: Si, Mn, Mg. EN AW-5182 is a Aluminum grade, while EN AW-6082 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.