Skip to content
Automated comparison Β· 43% overlap

EN AW-6063 vs EN AW-5083: 43% composition overlap. Significantly different materials serving different application areas.

EN AW-6063 vs EN AW-5083

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-6063

3.3206

Aluminum6xxx (Al-Mg-Si)

The most common extrusion alloy worldwide. Excellent surface finish, good corrosion resistance, and exceptional extrudability. The standard choice for architectural profiles (window frames, curtain walls, railings), heat sinks, and electrical enclosures.

EN AW-5083

3.3547

Aluminum5xxx_mg

The highest-strength non-heat-treatable aluminum alloy. Al-Mg4.5-Mn with outstanding seawater and industrial chemical resistance. Retains exceptional strength after welding (unlike 6xxx/7xxx). ASTM B928 certified for marine service. THE shipbuilding aluminum β€” also used for rail cars, pressure vessels, cryogenic tanks, truck bodies, and LNG applications. Available O, H111, H116, H321 tempers.

EN AW-6063EN AW-5083
Material Number3.32063.3547
CategoryAluminumAluminum
StandardEN 573-3EN 485-2

Chemical composition (wt%)

ElementEN AW-6063EN AW-5083Overlap
Si0.2–0.6%0–0.4%Partial
Mn0–0.1%0.4–1%No overlap
Cr0–0.1%0.05–0.25%Partial
Cu0–0.1%0–0.1%OK

Mechanical properties

PropertyEN AW-6063EN AW-5083Unit
tensile_strengthβ‰₯ 215270–345MPa
yield_strengthβ‰₯ 170115–130MPa
elongationβ‰₯ 8β‰₯ 16%

Compatibility Assessment

EN AW-6063 and EN AW-5083 have significantly different compositions (43% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-6063 the same as EN AW-5083?

EN AW-6063 and EN AW-5083 have a 43% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-6063 with EN AW-5083?

Generally not recommended. The compositions differ significantly (43% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-6063 and EN AW-5083?

The main differences are in the following elements: Si, Mn, Cr, Mg. EN AW-6063 is a Aluminum grade, while EN AW-5083 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.