Skip to content
Automated comparison Β· 50% overlap

EN AW-6063 vs EN AW-6082: 50% composition overlap. Moderate differences, generally not direct substitutes.

EN AW-6063 vs EN AW-6082

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-6063

3.3206

Aluminum6xxx (Al-Mg-Si)

The most common extrusion alloy worldwide. Excellent surface finish, good corrosion resistance, and exceptional extrudability. The standard choice for architectural profiles (window frames, curtain walls, railings), heat sinks, and electrical enclosures.

EN AW-6082

3.2315

Aluminum6xxx_mg_si

THE European structural aluminum alloy β€” AlSi1MgMn. Highest strength in the 6xxx series (UTS 310 T6). Excellent machinability, good weldability (but HAZ softening), and good corrosion resistance. THE default choice for structural aluminum in Europe β€” equivalent to what 6061 is in the US. Used for bridges, cranes, transport structures, offshore, and machined components.

EN AW-6063EN AW-6082
Material Number3.32063.2315
CategoryAluminumAluminum
StandardEN 573-3EN 755-2

Chemical composition (wt%)

ElementEN AW-6063EN AW-6082Overlap
Si0.2–0.6%0.7–1.3%No overlap
Mn0–0.1%0.4–1%No overlap
Cr0–0.1%0–0.25%OK
Cu0–0.1%0–0.1%OK

Mechanical properties

PropertyEN AW-6063EN AW-6082Unit
tensile_strengthβ‰₯ 215290–340MPa
yield_strengthβ‰₯ 170250–290MPa
elongationβ‰₯ 88–10%

Compatibility Assessment

EN AW-6063 and EN AW-6082 have moderate differences (50% overlap). They are generally not direct substitutes. Consider the specific requirements of your application.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-6063 the same as EN AW-6082?

EN AW-6063 and EN AW-6082 have a 50% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-6063 with EN AW-6082?

Generally not recommended. The compositions differ significantly (50% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-6063 and EN AW-6082?

The main differences are in the following elements: Si, Mn, Mg. EN AW-6063 is a Aluminum grade, while EN AW-6082 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.