Skip to content
Automated comparison Β· 56% overlap

EN AW-6082 vs EN AW-6101: 56% composition overlap. Moderate differences, generally not direct substitutes.

EN AW-6082 vs EN AW-6101

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-6082

3.2315

Aluminum6xxx (Al-Mg-Si)

High-strength structural aluminium alloy in the Al-Mg-Si family. One of the strongest 6xxx series alloys due to manganese addition. Replaced 6061 in many European applications. Used for trusses, bridges, cranes, transport, scaffolding, and marine applications. Heat treatable (T6/T651).

EN AW-6101

EN AW-6101

Aluminum6xxx_al_mg_si

Al-Mg-Si electrical conductor alloy β€” optimized for maximum electrical conductivity (56-57% IACS T6) while maintaining moderate strength. THE aluminum busbar and power cable alloy. Used for high-voltage busbars, electrical conductors, overhead transmission lines, transformer windings, and switchgear. Replaces copper at 1/3 the weight and lower cost per amp-meter.

EN AW-6082EN AW-6101
Material Number3.2315EN AW-6101
CategoryAluminumAluminum
StandardEN 573-3EN 573-3

Chemical composition (wt%)

ElementEN AW-6082EN AW-6101Overlap
Si0.7–1.3%0.3–0.7%Partial
Mn0.4–1%β€”β€”
Cr0–0.25%β€”β€”
Cu0–0.1%0–0.1%OK

Mechanical properties

PropertyEN AW-6082EN AW-6101Unit
tensile_strengthβ‰₯ 310200–240MPa
yield_strengthβ‰₯ 260170–200MPa
elongationβ‰₯ 810–15%

Compatibility Assessment

EN AW-6082 and EN AW-6101 have moderate differences (56% overlap). They are generally not direct substitutes. Consider the specific requirements of your application.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-6082 the same as EN AW-6101?

EN AW-6082 and EN AW-6101 have a 56% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-6082 with EN AW-6101?

Generally not recommended. The compositions differ significantly (56% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-6082 and EN AW-6101?

The main differences are in the following elements: Si, Mg. EN AW-6082 is a Aluminum grade, while EN AW-6101 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.