EN AW-5754 vs EN AW-6082: 55% composition overlap. Moderate differences, generally not direct substitutes.
EN AW-5754 vs EN AW-6082
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5754
3.3535
Medium-strength non-heat-treatable aluminium alloy with good corrosion resistance and excellent weldability. Lower Mg than 5083 for better formability. The standard alloy for automotive body panels (inner), chemical equipment, and food industry applications.
EN AW-6082
3.2315
High-strength structural aluminium alloy in the Al-Mg-Si family. One of the strongest 6xxx series alloys due to manganese addition. Replaced 6061 in many European applications. Used for trusses, bridges, cranes, transport, scaffolding, and marine applications. Heat treatable (T6/T651).
| EN AW-5754 | EN AW-6082 | |
|---|---|---|
| Material Number | 3.3535 | 3.2315 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-5754 | EN AW-6082 | Overlap |
|---|---|---|---|
| Si | 0β0.4% | 0.7β1.3% | No overlap |
| Mn | 0β0.5% | 0.4β1% | Partial |
| Cr | 0β0.3% | 0β0.25% | OK |
| Cu | 0β0.1% | 0β0.1% | OK |
Mechanical properties
| Property | EN AW-5754 | EN AW-6082 | Unit |
|---|---|---|---|
| tensile_strength | 190β240 | β₯ 310 | MPa |
| yield_strength | β₯ 80 | β₯ 260 | MPa |
| elongation | β₯ 17 | β₯ 8 | % |
Compatibility Assessment
EN AW-5754 and EN AW-6082 have moderate differences (55% overlap). They are generally not direct substitutes. Consider the specific requirements of your application.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5754 the same as EN AW-6082?
EN AW-5754 and EN AW-6082 have a 55% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5754 with EN AW-6082?
Generally not recommended. The compositions differ significantly (55% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5754 and EN AW-6082?
The main differences are in the following elements: Si, Mn, Mg. EN AW-5754 is a Aluminum grade, while EN AW-6082 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.