EN AW-6082 vs EN AW-5052: 27% composition overlap. Significantly different materials serving different application areas.
EN AW-6082 vs EN AW-5052
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-6082
3.2315
High-strength structural aluminium alloy in the Al-Mg-Si family. One of the strongest 6xxx series alloys due to manganese addition. Replaced 6061 in many European applications. Used for trusses, bridges, cranes, transport, scaffolding, and marine applications. Heat treatable (T6/T651).
EN AW-5052
EN AW-5052
General-purpose Al-Mg alloy β Mg 2.2-2.8%. Good balance of formability, corrosion resistance, and moderate strength (UTS 210-260 H32). Non-heat-treatable β strengthened by cold work. THE most widely used 5xxx alloy globally by tonnage. Used for sheet metal work, fuel tanks, marine components, appliances, lighting, and general fabrication. Excellent weldability.
| EN AW-6082 | EN AW-5052 | |
|---|---|---|
| Material Number | 3.2315 | EN AW-5052 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-6082 | EN AW-5052 | Overlap |
|---|---|---|---|
| Si | 0.7β1.3% | 0β0.25% | No overlap |
| Mn | 0.4β1% | β | β |
| Cr | 0β0.25% | 0.15β0.35% | Partial |
| Cu | 0β0.1% | β | β |
Mechanical properties
| Property | EN AW-6082 | EN AW-5052 | Unit |
|---|---|---|---|
| tensile_strength | β₯ 310 | 210β260 | MPa |
| yield_strength | β₯ 260 | 160β210 | MPa |
| elongation | β₯ 8 | 7β12 | % |
Compatibility Assessment
EN AW-6082 and EN AW-5052 have significantly different compositions (27% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-6082 the same as EN AW-5052?
EN AW-6082 and EN AW-5052 have a 27% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-6082 with EN AW-5052?
Generally not recommended. The compositions differ significantly (27% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-6082 and EN AW-5052?
The main differences are in the following elements: Si, Cr, Mg. EN AW-6082 is a Aluminum grade, while EN AW-5052 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.